Casting hlau fittings feem ntau ua rau ntau yam tsis xws luag hauv kev tsim khoom. Tam sim no Shijiazhuang donghuan malleable hlau technology co., ltd qhia koj yuav ua li cas los tiv thaiv xws li tsis xws luag yeej ib txwm muaj teeb meem uas casting manufacturers muaj kev txhawj xeeb txog.
Lub rhiav ntau lawm mas siv cov tsoos ntsuab xuab zeb casting txheej txheem los tsim steel castings. Nyob rau hauv lub sij hawm ntev ntau lawm, nws pom tau hais tias cov nram qab no tsis xws luag yuav tshwm sim nyob rau hauv lub steel castings, xws li xuab zeb qhov, sticking xuab zeb, pores, qhov, xuab zeb inclusion thiab caws pliav, o, xuab zeb no.
1. Kev tiv thaiv kab mob trachoma:
(1) nruj me ntsis tswj kev ua haujlwm ntawm molding xuab zeb;
(2) Ua ntej kaw lub thawv, daws cov xuab zeb ntab saum npoo ntawm cov pwm concave thiab cov xuab zeb core kom huv si thiab ruaj khov kaw lub thawv;
(3) Teem kom tsim nyog thiab siv tau zoo pouring system software;
(4) txheej txheej ntawm lub khob ncuav yuav tsum du thiab huv si, thiab tsis tuaj yeem muaj cov xuab zeb ntab.
2. Kev tiv thaiv kev tiv thaiv cov xuab zeb
(1) Siv xuab zeb nrog hluav taws kub;
(2) Txo qhov kub thiab txias thiab nce tus nqi pouring;
(3) Lub compactness ntawm cov xuab zeb pwm yuav tsum siab (feem ntau ntau tshaj 85) thiab zoo-proportioned;
(4) Xaiv cov architectural txheej uas tsis tawg ntawm qhov kub thiab txias thiab tsis txhob sinter rau hauv molten qhov.
Txais tos rau sab laj peb lub tuam txhab rau ntau yam teeb meem casting.